Send Message
Home ProductsCalcium Formate

CAS 544-17-2 Calcium Salt Of Formic Acid

Certification
China Shandong Jufu Chemical Technology Co., Ltd. certification
China Shandong Jufu Chemical Technology Co., Ltd. certification
Customer Reviews
Received the sample from your company, which is very suitable for the concrete additives required by our factory, so we ordered a large number of products, it is a pleasant cooperation!

—— John Simmers

This is an old partner of our company! I've been ordering water reducer here for a long time, it's a trusted company, the ingredients are pure, and the product specifications I need are met.

—— Yogananda Muthaiah

The product content is high,the price is reasonable,already put into use,the cooperation is happy.

—— ZMUS.PAKE

Many thanks to the workers who handled the packing of the pce liquid and lignin ,and to you of course. Packed very well.We have started work!

—— Josephine

I'm Online Chat Now

CAS 544-17-2 Calcium Salt Of Formic Acid

CAS 544-17-2 Calcium Salt Of Formic Acid
CAS 544-17-2 Calcium Salt Of Formic Acid

Large Image :  CAS 544-17-2 Calcium Salt Of Formic Acid

Product Details:
Place of Origin: China
Brand Name: Jufu Chemical
Model Number: Calcium Formate
Payment & Shipping Terms:
Minimum Order Quantity: 1ton
Price: USD1400-1500/MT
Packaging Details: 25kg/bag,20GP/25MT with pallet
Delivery Time: 5 working days
Payment Terms: L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability: 3000TON/MONTH
Detailed Product Description
Main Name: Formic Acid CAS: CAS 544-17-2
Feature: Anhydrous Usage: Building Concrete
Moisture: 0.5% Shape: Powder
PH Value(10% Solutedwater): 6.5-7.5 Ca: 30%
High Light:

Ca 30% calcium salt of formic acid

,

CAS 544-17-2 calcium salt of formic acid

,

PH 6.5 formic acid salt

Anhydrous Formic Acid Calcium Special For Building Concrete CAS 544-17-2

 

JF CALCIUM FORMATE Product Description:

 

Synonym: CAS 544-17-2

 

Calcium formate is a kind of additive which has no erosive effect on steel bar. Its molecular formula is C2H2CaO4, which mainly accelerates the hydration of calcium silicate in cement and increases the early strength of cement mortar. The influence of calcium formate on strength of cement mortar mainly depends on the content of tricalcium silicate in cement. Tricalcium silicate is less, it will not attenuate the late strength of cement mortar, and there is a certain antifreeze at low temperature.

 

ITEMS

SPECIFICATIONS

Calsium Formate 98%
Purity ≥98%
Water Insoluble ≤0.2%
PH Value(10% Solutedwater) 6.5-7.5
Ca 30%
Appearance White Crystals
Moisture 0.5%
Weight Loss At Drying ≤0.5%

 

CAS 544-17-2 Calcium Salt Of Formic Acid 0

 

There are two main reasons for adding early strength agent to polymer mortar:


One is that some construction sites require a certain amount of construction, which should be strengthened earlier on the basis of early strength to meet the requirements of outdoor force. Second, when the temperature is low, the strength of the mortar slows down and will be affected. The strength of the mortar is low when it freezes. The more the mortar is beaten, the mortar will be frozen in the early low-strength period, so add the early strength agent at low temperature.


At low temperatures, even the addition of strength agents will reduce the strength of cement mortar. One is because the water conversion rate is slow when construction is performed in a low temperature environment, which affects the construction efficiency. When the temperature reaches the freezing point, the water turns into ice and expands in volume, making it easy to hollow out and fall off. After the two people went deep inside, the strength of the mortar was significantly reduced. During construction, icing occurred.


Naturally, the hydration reaction is a release, with a certain hydration temperature, the cement strength is reduced. If the welding temperature exceeds 0°C, the hydration reaction will continue and the strength of the once-cycle cement will decrease. The third is the general reheatable reaction powder reaction powder reaction. The molding temperature of EVA is above 0°C, while the temperature of EVA products is above 0°C, generally around 0°C. gender. Moreover, when the temperature is slow, the dissolution rate of salt particles is slower, and the adhesion and workability of the mortar are weaker. Therefore, the construction quality above 5°C can be guaranteed.

 

Jufu Company:

 

In its long-term business activities, Shandong Jufu Chemical Co., Ltd. always insists that quality responsibility is more important than Mount Tai. Quality is the life of an enterprise and the guarantee of its competitiveness. Observing the principle of equality and mutual benefit, respecting contracts and keeping credibility, we have established a good corporate image and reputation in the industry. We wholeheartedly welcome new and old friends at home and abroad, and friendly businessmen to visit our company to guide and negotiate business, work together and prosper the future.

 

CAS 544-17-2 Calcium Salt Of Formic Acid 1

 

Contact Details
Shandong Jufu Chemical Technology Co., Ltd.

Contact Person: Ms. SHANSONG JUFU CHEM TECH

Tel: 86-053188987705

Fax: 86-0531-8898-7710

Send your inquiry directly to us (0 / 3000)